  • Standard Practice for Elevated Temperature and Moisture Conditioning of Pultruded Fiber Reinforced Polymer (FRP) Composites Used in Structural Designs
  • standard by ASTM International, 09/01/2015
  • Publisher: ASTM

$20.00$39.00


1.1 In general, it is feasible that the mechanical properties of FRP composites will be affected by environmental conditions such as exposure to moisture at elevated temperatures. In order to make reliable comparisons between different materials under elevated temperature and moisture environmental conditions, it is necessary to standardize the elevated temperature and moisture conditions to which specimens of these materials are subjected prior to and during testing. This practice defines procedures for elevated temperature and moisture conditioning of pultruded FRP composites intended for use in structural design applications. The conditioning medium representing elevated temperature and moisture exposure described in this standard practice is distilled water maintained at 37.8 ± 1.5°C (100 ± 3°F) for 1000 hours.

Related Products

ASTM D4138-07a(2013)

ASTM D4138-07a(2013)

Standard Practices for Measurement of Dry Film Thickness of Protective Coating Systems by De..

$22.00 $44.00

ASTM B594-06

ASTM B594-06

Standard Practice for Ultrasonic Inspection of Aluminum-Alloy Wrought Products for Aerospace Applica..

$26.00 $52.80

ASTM E2422-11

ASTM E2422-11

Standard Digital Reference Images for Inspection of Aluminum Castings..

$22.00 $44.00

ASTM A773/A773M-01(2009)

ASTM A773/A773M-01(2009)

Standard Test Method for dc Magnetic Properties of Materials Using Ring and Permeameter Procedures w..

$26.00 $52.80