1.1 This procedure is used to define the papermaking quality of pulp, by subjecting it to a controlledmechanical treatment in a laboratory beater; see also TAPPI T248 "Laboratory Beating of Pulp (PFI Mill Method)."

1.2 The beating procedure may be used with any pulp, suitably modifying the withdrawal schedule to providethe number of samples required for a satisfactory beater curve. The method may not give satisfactory results with certain extremely long-fibered pulps, such as cotton fibers or jute since the fibers entangle and tend to rope in the beater.

Related Products

TAPPI T 441 om-09

TAPPI T 441 om-09

Water Absorptiveness of Sized (Non-bibulous) Paper, Paperboard, and Corrugated Fiberboard (Cobb Test..

$27.00 $54.00

TAPPI T825 om-03

TAPPI T825 om-03

Flat Crush Test of Corrugated Board (Rigid Support Method)..

$45.00 $90.00

TAPPI TIP0607-09

TAPPI TIP0607-09

Solubility of Sulfur Dioxide in Magnesium Bisulfite Solution..

$25.00 $49.00

TAPPI T512 sp-12

TAPPI T512 sp-12

Creasing of Flexible Packaging Material Paper Specimens for Testing..

$25.00 $49.00